dc.creatorLima-Corrêa, Renata A. B.-
dc.creatorCastro, Cínthia S.-
dc.creatorAssaf, José M.-
dc.date.accessioned2019-06-07T10:31:17Z-
dc.date.available2019-06-07T10:31:17Z-
dc.date.issued2018-
dc.identifier.citationLIMA-CORRÊA, R. A. B.; CASTRO, C. S.; ASSAF, J. M. Lithium containing MgAl mixed oxides obtained from sol-gel hydrotalcite for transesterification. Brazilian Journal of Chemical Engineering, São Paulo, v. 35, n. 1, p. 189 - 195, Jan./Mar. 2018.pt_BR
dc.identifier.urihttp://repositorio.ufla.br/jspui/handle/1/34678-
dc.description.abstractThe innumerous advantages of heterogeneous catalysts employed in biodiesel production have stimulated the search for a solid catalyst capable of replacing the industrially used homogeneous catalysts. This paper investigates the effect of the sol-gel method in the catalytic activity and stability of Li-MgAl mixed oxides prepared by the “in situ” lithium addition to a MgAl hydrotalcite. The analyses based on N2 physisorption, thermogravimetric analysis, X-ray diffractometry, scanning electron microscopy and temperature-programmed desorption of CO2 were carried out to elucidate the properties of the catalysts. Considerable differences in the physico-chemical properties of the catalysts were observed with the Li addition. Li reduced the surface area and increased the crystallite size of the oxides. Furthermore, Li-MgAl mixed oxides prepared by the calcination of the sol-gel MgAl hydrotalcites presented substantial morphological differences when compared to the same oxides obtained by heat treatment of hydrotalcites synthesized via the conventional co-precipitation route. Furthermore, Li increased the number and strength of the base sites which resulted in the increase of the oxide reactivities towards the transesterification reaction between methyl acetate and ethanol. The activity was dependent on the Li loading on the catalysts. The catalyst containing only 5 wt.% Li turned out to be highly active (( 85% conversion at 50°C, ethanol/methyl acetate molar ratio = 6/1, 4 wt.% of catalyst and 30 min of reaction). Stability tests showed that the Li-MgAl catalysts lose activity after 3 reuse cycles.pt_BR
dc.languageen_USpt_BR
dc.publisherBrazilian Society of Chemical Engineeringpt_BR
dc.rightsAttribution 4.0 International*
dc.rightsacesso abertopt_BR
dc.rights.urihttp://creativecommons.org/licenses/by/4.0/*
dc.sourceBrazilian Journal of Chemical Engineeringpt_BR
dc.subjectHydrotalcitept_BR
dc.subjectSol-gel methodpt_BR
dc.subjectTransesterificationpt_BR
dc.subjectLithiumpt_BR
dc.subjectMixed oxidept_BR
dc.subjectHeterogeneous catalysispt_BR
dc.titleLithium containing MgAl mixed oxides obtained from sol-gel hydrotalcite for transesterificationpt_BR
dc.typeArtigopt_BR
Aparece nas coleções:DEG - Artigos publicados em periódicos

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
ARTIGO_Lithium containing MgAl mixed....pdf1,59 MBAdobe PDFVisualizar/Abrir


Este item está licenciada sob uma Licença Creative Commons Creative Commons