Título: Qualidade de moirões tratados com diferentes concentrações de CCA-C
Título(s) alternativo(s): Treated posts quality with different CCA-C concentrations
Autores: Silva, José Reinaldo Moreira da
Baraúna, Edy Eime Pereira
Hein, Paulo Ricardo Gherardi
Silva, José Reinaldo Moreira da
Baraúna, Edy Eime Pereira
Oliveira, Leandro Silva de
Trugilho, Paulo Fernando
Palavras-chave: Madeira – Conservação
Madeira – Permeabilidade
Wood – Conservation
Wood – Permeability
Data do documento: 31-Mai-2017
Editor: Universidade Federal de Lavras
Citação: BRITO, T. R. Qualidade de moirões tratados com diferentes concentrações de CCA-C. 2017. 41 p. Dissertação (Mestrado em Ciência e Tecnologia da Madeira)-Universidade Federal de Lavras, Lavras, 2017.
Resumo: This study aimed reduce CCA concentration established by NBR 9480 (ABNT, 2009), without affecting the quality of treated posts. Eucalyptus cloeziana (seminal origin) and E. urophylla x E. camaldulensis (clonal hybrid) from commercial plantations, at the age of six years were used. 25 posts with length of 2.20 m and diameter of 8 to 10 cm, randomly collected in drying cells were picked for each genetic material. The basic density, moisture, sapwood percentage and the treatable volume were determined, besides characterizing anatomical structure. The materials were treated with concentrations of 1.2%, 1.3%, 1.4%, 1.5% and 1.6% of CCA-C active ingredients. The quality of the preservative treatment was evaluated by means of penetration and retention and toxicity (treated wood) to termites by means of food preference test with Nasutitermes corniger Motsch. The treated wood of E. cloeziana presented 44% of the posts with partial and regular penetration, 40% with partial and irregular penetration, 12% with deep and irregular penetration and 4% with zero penetration. The clonal hybrid presented 68% of the posts with deep and regular penetration, 24% with deep and irregular penetration and 8% as partial and regular penetration. The concentrations of 1.4, 1.5% and 1.4, 1.6% of active ingredients for, respectively, E. cloeziana and clonal hybrid reached the minimum retention according to NBR 9480 (ABNT, 2009). In both genetic materials, the highest values of mass loss were in the controls that did not receive preservative treatment. The damage on both genetic materials was classified as "undamaged, allowing superficial scarifications".
URI: http://repositorio.ufla.br/jspui/handle/1/13084
Aparece nas coleções:Ciência e Tecnologia da Madeira - Mestrado (Dissertações)

Arquivos associados a este item:
Arquivo Descrição TamanhoFormato 
DISSERTAÇÃO_Qualidade de moirões tratados com diferentes concentrações de CCA-C.pdf1,82 MBAdobe PDFVisualizar/Abrir


Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.